Report on calibration of the participating laboratories

The report describes the results of an intercomparison test of the laboratories participating in the Crevcorr-project. The Critical Crevice Temperature (CCT) of the 2205 duplex and the 254SMO super austenitic stainless steel was determined by several laboratories according to a well defined procedure. Rectungal coupons were equipped with multi-crevice-washers and exposed in a ferric chloride solution at three different temperatures, after which the resulting attack was noted. Amongst the possible criteria, it would appear that a maximum depth of attack equalling or exceeding 25 µm allows a relatively accurate determination of CCT, even though significant scatter exists between individual depth results from different laboratories and in some cases between duplicate tests.

Kontakt

Sytze HUIZINGA, (Senior Corrosion Engineer)
Tel.: +31-20-6302449
Fax: +31-20-6302989
E-Mail-Adresse
Folgen Sie uns auf: RSS Facebook Twitter YouTube Verwaltet vom Amt für Veröffentlichungen der EU Nach oben