{"contenttype":"article","language":"fr","availableLanguages":"de,en,es,fr,it,pl","rcn":"190977","id":"190977-new-superalloys-for-highefficiency-jet-engines","title":"De nouveaux superalliages pour des r\u00e9acteurs \u00e0 haut rendement","teaser":"Capables de r\u00e9sister \u00e0 l\u0027\u00e9norme chaleur produite par les r\u00e9acteurs, l\u00e0 o\u00f9 les autres mat\u00e9riaux c\u00e8deraient, les \u00absuper pouvoirs\u00bb des superalliages permettent aux avions de voler. Des scientifiques financ\u00e9s par l\u0027UE ont \u00e9tudi\u00e9 une nouvelle g\u00e9n\u00e9ration de superalliages \u00e0 base de nickel qui devraient permettre une augmentation de la temp\u00e9rature de fonctionnement des r\u00e9acteurs, et donc leur efficacit\u00e9.","body":"\u003Csection\u003E\u003CsectionBody\u003ELes temp\u00e9ratures \u00e0 l\u0027int\u00e9rieur des moteurs d\u0027avion peuvent d\u00e9passer le point de fusion des m\u00e9taux, mais les propri\u00e9t\u00e9s exceptionnelles de certains mat\u00e9riaux leur permettent de fonctionner. Combinant r\u00e9sistance m\u00e9canique, r\u00e9sistance \u00e0 la d\u00e9formation due au fluage thermique, bonne stabilit\u00e9 de surface et r\u00e9sistance \u00e0 la corrosion ou \u00e0 l\u0027oxydation, les superalliages sont g\u00e9n\u00e9ralement con\u00e7us pour \u00eatre utilis\u00e9s \u00e0 des temp\u00e9ratures \u00e9lev\u00e9es.\n\nComme pour tout autre mat\u00e9riau, les propri\u00e9t\u00e9s des superalliages sont fortement influenc\u00e9es par leur microstructure, elle-m\u00eame d\u00e9termin\u00e9e par leur composition et le traitement qu\u0027ils ont subi. Dans le projet NECTAR (New generation of NiAl-based eutectic composites with tuneable properties), financ\u00e9 par l\u0027UE, des scientifiques ont men\u00e9 des \u00e9tudes sur des composites \u00e0 base de superalliages nickel-aluminure (NiAl), en associant des calculs de thermodynamique de pointe avec des concepts avanc\u00e9s de conception et de traitement.\n\n\u00c0 leur point eutectique, les diff\u00e9rents composants d\u0027un m\u00e9lange sont dans des phases diff\u00e9rentes (liquide, alpha et b\u00eata) qui se trouvent toutes en \u00e9quilibre. L\u0027accent a \u00e9t\u00e9 mis sur les compositions d\u0027un m\u00e9lange contenant quatre composants tels que le nickel, l\u0027aluminium, le chrome, le tungst\u00e8ne, le rh\u00e9nium et le vanadium. Apr\u00e8s avoir recueilli toutes les informations exp\u00e9rimentales sur les diagrammes de phase quaternaire et les propri\u00e9t\u00e9s thermodynamiques de chaque phase, les scientifiques ont cr\u00e9\u00e9 des bases de donn\u00e9es thermodynamiques pour les trois phases des diff\u00e9rents syst\u00e8mes quaternaires possibles.\n\nApr\u00e8s avoir s\u00e9lectionn\u00e9 deux syst\u00e8mes eutectiques, l\u0027\u00e9quipe a d\u00e9velopp\u00e9 des cartes structurelles et d\u00e9fini la composition des phases. Les scientifiques ont d\u00e9velopp\u00e9 des mod\u00e8les de diffusion et de phase de champs pour mod\u00e9liser le processus de solidification des alliages eutectiques. Ils ont \u00e9galement mod\u00e9lis\u00e9 la microstructure, la morphologie de la croissance, la r\u00e9gularit\u00e9 et l\u0027uniformit\u00e9 des syst\u00e8mes eutectiques.\n\nEnfin, l\u0027\u00e9quipe a d\u00e9crit la d\u00e9pendance des propri\u00e9t\u00e9s m\u00e9caniques \u00e0 la temp\u00e9rature comme une fonction de la fraction volumique de la phase de renforcement, de la r\u00e9sistance \u00e0 la rupture et des m\u00e9canismes de d\u00e9faillance, ainsi que les propri\u00e9t\u00e9s de fluage des syst\u00e8mes eutectiques. Les alliages pr\u00e9sentant une plus faible fraction volumique de fibres se sont r\u00e9v\u00e9l\u00e9s \u00eatre plus solides et avoir une meilleure r\u00e9sistance au fluage, alors que les alliages ayant une fraction volumique plus \u00e9lev\u00e9e se sont montr\u00e9s plus ductiles et plus r\u00e9sistants \u00e0 la rupture.\n\nNECTAR a cibl\u00e9 une nouvelle g\u00e9n\u00e9ration de composites \u00e0 base de NiAl dot\u00e9s de propri\u00e9t\u00e9s ajustables, pr\u00e9sentant de meilleures performances que les meilleurs alliages \u00e0 base de nickel actuels, et capables de r\u00e9sister \u00e0 des temp\u00e9ratures sup\u00e9rieures \u00e0 1 150\u00b0C, qu\u0027atteignent g\u00e9n\u00e9ralement les moteurs \u00e0 r\u00e9action.\u003C\/sectionBody\u003E\u003C\/section\u003E","keywords":"Superalliages, moteurs \u00e0 r\u00e9action, NECTAR, eutectique, nickel-aluminure, thermodynamique","contentCreationDate":"2017-02-01 11:42:36","contentUpdateDate":"2017-02-01 11:42:29","lastUpdateDate":"2017-02-01 11:42:52","archivedDate":"2024-06-10 00:00:00","relations":{"categories":[{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"indust","title":"Technologies industrielles","displayCode":"\/Technologies industrielles","attributes":{"classification":"applicationDomain","type":"isApplicableIn"}},{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"brief","title":"R\u00e9sultat en bref","description":"Article: classique et am\u00e9lior\u00e9","displayCode":"\/R\u00e9sultat en bref","attributes":{"classification":"collection","type":"belongsTo"}},{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"editorial","title":"\u00c9ditorial CORDIS","description":"R\u00e9dig\u00e9 par CORDIS","displayCode":"\/\u00c9ditorial CORDIS","attributes":{"classification":"source","type":"isProvidedBy"}}],"associations":[{"availableLanguages":"en","rcn":"102697","id":"303409","acronym":"NECTAR","archivedDate":"2024-06-18 00:00:00","relations":{"categories":[{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"project","title":"Projet","description":"Fiches d\u0027information du projet","displayCode":"\/Projet","attributes":{"classification":"collection","type":"belongsTo"}},{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"\/25\/63\/387","title":"composites","displayCode":"\/ing\u00e9nierie et technologie\/ing\u00e9nierie des materiaux\/composites","attributes":{"classification":"euroSciVoc","type":"isInFieldOfScience"}},{"language":"fr","availableLanguages":"en","code":"MC-CIG","attributes":{"classification":"projectFundingSchemeCategory","type":"relatedProjectFundingSchemeCategory"}},{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"corda","title":"CORDA","description":"Centrale de donn\u00e9es de la recherche RTD","displayCode":"\/CORDA","attributes":{"classification":"source","type":"isProvidedBy"}}],"associations":[{"availableLanguages":"de,en,es,fr,it,pl","rcn":"848","code":"FP7-PEOPLE","frameworkProgramme":"FP7","pga":"FP7-PEOPLE","title":"Programme sp\u00e9cifique \u0022Personnes\u0022 mettant en \u0153uvre le septi\u00e8me programme-cadre de la Communaut\u00e9 europ\u00e9enne pour des activit\u00e9s de recherche, de d\u00e9veloppement technologique et de d\u00e9monstration (2007-2013)","shortTitle":"Programme sp\u00e9cifique \u0022Personnes\u0022","parent":{"rcn":"1401\/837","code":"EC\/FP7"},"archivedDate":"2024-06-12 00:00:00","relations":{"categories":[{"language":"fr","code":"legalbasis","title":"Base juridique","description":"Programme: Base juridique pour le financement de la recherche","displayCode":"\/Base juridique","attributes":{"classification":"collection","type":"belongsTo"}},{"language":"fr","code":"editorial","title":"\u00c9ditorial CORDIS","description":"R\u00e9dig\u00e9 par CORDIS","displayCode":"\/\u00c9ditorial CORDIS","attributes":{"classification":"source","type":"isProvidedBy"}}]},"contenttype":"programme","attributes":{"source":"corda","type":"relatedLegalBasis"}},{"availableLanguages":"en","rcn":"15136","code":"FP7-PEOPLE-2011-CIG","frameworkProgramme":"FP7","parent":{"rcn":"10053\/11419\/848\/1401\/837","code":"PEOPLE-2\/PEOPLE\/FP7-PEOPLE\/EC\/FP7"},"archivedDate":"2024-06-14 00:00:00","relations":{"categories":[{"language":"fr","code":"topic","title":"Th\u00e8me","description":"Programme: Partie du programme de travail de la Commission mettant en \u0153uvre la base juridique","displayCode":"\/Th\u00e8me","attributes":{"classification":"collection","type":"belongsTo"}},{"language":"fr","code":"editorial","title":"\u00c9ditorial CORDIS","description":"R\u00e9dig\u00e9 par CORDIS","displayCode":"\/\u00c9ditorial CORDIS","attributes":{"classification":"source","type":"isProvidedBy"}}]},"contenttype":"programme","attributes":{"source":"corda","type":"relatedTopic"}}]},"contenttype":"project","attributes":{"source":"editorial","type":"relatedProject"}},{"availableLanguages":"en","rcn":"187020","archivedDate":"2024-06-23 00:00:00","relations":{"categories":[{"language":"fr","code":"pubsum","title":"R\u00e9sum\u00e9 du rapport","description":"R\u00e9sultat: R\u00e9sum\u00e9 publiable (FP7 SESAM) et R\u00e9sum\u00e9 soumis \u00e0 la publication (H2020 SyGMa)","displayCode":"\/R\u00e9sum\u00e9 du rapport","attributes":{"classification":"collection","type":"belongsTo"}},{"language":"fr","code":"sesam","title":"SESAM","description":"Syst\u00e8me de rapport de RTD du 7e PC (dont Marie Curie du 6e PC)","displayCode":"\/SESAM","attributes":{"classification":"source","type":"isProvidedBy"}}],"associations":[{"rcn":"102697","id":"303409","relations":{"categories":[{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"project","title":"Projet","description":"Fiches d\u0027information du projet","displayCode":"\/Projet","attributes":{"classification":"collection","type":"belongsTo"}},{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"\/25\/63\/387","title":"composites","displayCode":"\/ing\u00e9nierie et technologie\/ing\u00e9nierie des materiaux\/composites","attributes":{"classification":"euroSciVoc","type":"isInFieldOfScience"}},{"language":"fr","availableLanguages":"en","code":"MC-CIG","attributes":{"classification":"projectFundingSchemeCategory","type":"relatedProjectFundingSchemeCategory"}},{"language":"fr","availableLanguages":"de,en,es,fr,it,pl","code":"corda","title":"CORDA","description":"Centrale de donn\u00e9es de la recherche RTD","displayCode":"\/CORDA","attributes":{"classification":"source","type":"isProvidedBy"}}]},"contenttype":"project","attributes":{"source":"sesam","type":"relatedProject"}}]},"contenttype":"result","attributes":{"source":"editorial","type":"relatedResult"}},{"language":"fr","availableLanguages":"de,en,es,fr,it,pl,any","uri":"\/docs\/results\/images\/2017-01\/190977.jpg","mimetype":"image\/jpeg","size":"0","copyright":"\u00a9 Christian Lagerek, Shutterstock","contenttype":"webItem","attributes":{"represents":"article","source":"editorial","type":"relatedImage"}}],"regions":[{"name":"Espagne","rcn":"242387496","nutsCode":"ES","euCode":"ES","isoCode":"ES","attributes":{"source":"editorial","type":"relatedRegion"}}]},"modelVersion":"132","icaVersion":"20.0.0-48f81e07"}