Obiettivo Use of low temperature waste heat for additional preheating of the combustion air and for prevention of low temperature corrosion. This technique yields an increase of the plant availability and a longer life of the recuperator by preventing the temperature from falling below the dew point to prevent corrosion.Innovative aspects : concept first realization.Long testing and measurement period to assess energy saving and efficiency and payback time.In industrial furnaces a part of the heat from the flue gas is used to pre-heat the combustion air. When intensive use is made of the heat from the flue gas, there is frequently a great drop in temperature to below the dew point. When the fuel gases are loaded with aggresive materials, the passing of the dew point causes low temperature corrosion on heat exchanger components. As a result of this, the heat exchanger is increasingly destroyed which entails constant worsening of efficiency very rare (once to twice per year) with some plants, i.e. reheating furnaces in the steel industry, so that more fuel is consumed over a long period because of defective air pre-heating insulation and the environment is thus burdened more than is required with an intact installation. A heat exchanger for a thermal capacity of 1.0 MW is to be erected upstream of the reheating furnace of a rolling mill fired by sulphur bearing coke oven gas. The energy for a pre-heating is taken from the skid rail cooling circuit which has a temperature level of maximum 90 deg. C Programma(i) ENG-ENDEMO C - Programme (EEC) of demonstration projects and industrial pilot projects (EEC) in the energy field, 1985-1989 Argomento(i) 3.4 - INDUSTRY Invito a presentare proposte Data not available Meccanismo di finanziamento DEM - Demonstration contracts Coordinatore Thyssen Stahl AG Contributo UE Nessun dato Indirizzo Kaiser-Wilhelm-Straße 100 47057 Duisburg Germania Mostra sulla mappa Costo totale Nessun dato