Objectif The aim of this project is to develop optimum hot and cold rolling and continuous annealing practices (steel compositions: 0.15% - 0.3% C; 0.8% - 2.0% Si; 0.8% - 2.0% Mn) to promote "Transformation Induced Plasticity" (TRIP) in which austenite is transformed into hard martensite by deformation. Laboratory and mill trials will be carried out, and final surface quality and welding properties checked. Programme(s) ECSC-STEELRES 8C - Medium-term guidelines (ECSC) for the programmes of technical steel research and of steel pilot/demonstration projects, 1991-1995 Thème(s) D3 - Physical metallurgy of rolling and finishing Appel à propositions Data not available Régime de financement CSC - Cost-sharing contracts Coordinateur THYSSEN STAHL Contribution de l’UE Aucune donnée Adresse Kaiser-Wilhelm-Strasse 100 47166 DUISBURG Allemagne Voir sur la carte Coût total Aucune donnée